fractography

fractography

美 [fræk'tɒgrəfɪ]  英 [fræk'tɒgrəfɪ]

  • n.金属断面显微镜观察
  • 网络断口金相;断口金相检验;断口金相学

英汉解释

n.
1.
金属断面显微镜观察

例句

fracture analysis of those bolts was conducted by means of macro examination , fractography and chemical composition analysis.

采用宏、微观检验和化学成分分析等方法对失效件进行了检测。

The fracture failure reasons of the hand-gear were analyzed by means of stress situation and fractography.

通过研究断裂时的应力状况及宏观断口,对手动小齿轮断裂失效原因进行了分析。

The microstructure and fractography of the samples were respectively observed by metallographic microscope and SEM.

利用金相显微镜、扫描电镜对试样的显微组织、断口形貌进行观察;

The fractography reveals that the alloy has high ductility because the dendritic phases produce in the alloy.

合金的断口分析结果表明,由于产生了塑性枝晶相,因此该合金具有较高塑性。

The scanning electron microscope(SEM)is employed to study sandstone fractography under thermo -mechanical coupling effects.

通过扫描电镜研究温度–拉应力共同作用下砂岩破坏的断口形貌。

Fractography Retroestimating Fatigue Stress and Its Application on Blade Fracture Analysis in Engineering

断口反推疲劳应力及其在叶片断裂分析中的应用

Standard Practice for Fractography and Characterization of Fracture Origins in Advanced Ceramics

高级陶瓷中断裂点的断口组织检查和特性的标准规程

Instability Fracture and Fractography Morphology of PMMA

PMMA的失稳断裂与断口形态